反应条件
polyvinylpyrrolidone in water Sonication; Ce(NO3)3 dissolved in water; KBF4 in water added; PVD added; mixt. stirred; exposed to high-intensity ultrasonic probe at room temp. in air for 80, 100, 120, 140 min; heated at 55°C; pptd.; ppt. washed with water, anhydrous ethanol; dried at 60°C for 12 h; XRD;
参考文献
Liu, Yang; Zhao, Yanbao; Yu, Laigui; Wu, Zhishen
Journal of Alloys and Compounds, 2009 , vol. 485, # 1-2 p. L1-L4