反应条件
in neat (no solvent) ball milled in ethanol with polyvinyl alcohol for 24 h, dried at 150 °C, ground, pressed into disks, sintered in Ar at 1500 °C for1 h at 10 °C heating and 5 °C cooling rates; <= 30 mol.percent Ti in starting mixture; powder XRD;
参考文献
Journal of the American Ceramic Society, , vol. 90, # 7 p. 2220 - 2225