反应条件
poly(ethylene glycol) (PEG); H2PtCl6*6H2O; N2H4*H2O in further solvent(s) electroless deposition; propyleneglycol as solvent; Co-salt and PEG dissolved when N2 bubbled, NaOH soln. added to pH 12, H2PtCl6 soln. added, N2H4 soln. added, stirred, placed in supercondcucting magnet for 1 h (1 -10 T); nanowires magnetically separated, ultrasonicated in ethanol for 10 min, washing repeated 10 times; detd. by XRD;
参考文献
Journal of the Electrochemical Society, , vol. 158, # 4 p. D210-D216