反应条件
in water byproducts: As; Electrolysis; Pt anode; ceramic or cation-exchange membrane; Cd, Cu, stainless steel, Sn, Ti, Ni, Pb cathode; j = 0.1-0.2 A/cm**2, at 14-50°C; electrolysis time: 0.5-3.0 h; optimal H3AsO4 concn. is 4-10 mol/l; chem. anal.;
参考文献
Smetanin; Smirnov; Chernykh; Turygin; Khudenko; Fedorov; Tomilov
Inorganic Materials, 2003 , vol. 39, # 1 p. 22 - 36