反应条件
in neat (no solvent) byproducts: C76, C78, C82; Electric Arc; packing core drilled graphite rods with Sc2O3, placing in electric arc reactor, filling with He at 300 Torr, introducing air flow at rate of 6 Torr/min, 220 A and 38 gap voltage were used; extn. (o-xylene) of soot, evapn., washing with ether or acetone, HPLC (toluene), UV;
参考文献
Journal of the American Chemical Society, , vol. 129, # 51 p. 16257 - 16262