hydrogen; 50 mass-percent MFI zeolite (38 Si/Al2 ratio) and aluminophosphate on alpha alumina core, containing 0.73 g of Mo per 100 g of MFI-aluminophosphate composition T=370 - 400°C; P=5168.02 Torr; 50 h; Product distribution / selectivity;
hydrogen; 65 weight percent of ZSM-23 molecular sieve (Si/Al2 ratio about 100) bound with 35 weight percent of alumina-rich binder T=500°C; P=750.075 Torr; Continuous reaction; Conversion of starting material;
conventional ZSM-5 zeolite prepared by crystallization of gel with molar composition Al2O3:9 TPA2O:1.25 Na2O:50 SiO2:385H2O in helium T=350 - 450°C; P=4560.31 Torr; Conversion of starting material;