反应条件
sodium hydroxide; acrylic acid sodium salt in water
pH of aq. soln. of Pt salt adjusted to 7.0 using dild. NaOH soln., purged with Ar, Na acrylate soln. added then H2 gas bubbled through soln. for30 min, flask sealed and stirred overnight in dark at room temp. (12 h); Pt nanoparticles obtained with acrylate capping, isolated by salt out method or centrifuged;
参考文献
Njoki, Peter N.; Jacob, Aisley; Khan, Bilal; Luo, Jin; Zhong, Chuan-Jian
Journal of Physical Chemistry B, 2006 , vol. 110, # 45 p. 22503 - 22509