Vournasos, A. C.
Comptes Rendus Hebdomadaires des Seances de l'Academie des Sciences, 1919 , vol. 168, p. 889 - 891
→
反应条件
in neat (no solvent)
Electrochem. Process; reaction under galvanostatic conditions in MSb2O6/Li cell at 20 °C; detd. by HRTEM, XRD;
参考文献
Larcher; Prakash; Laffont; Womes; Jumas; Olivier-Fourcade; Hedge; Tarascon
Journal of the Electrochemical Society, 2006 , vol. 153, # 9 p. A1778-A1787
→
反应条件
in neat (no solvent)
samples crushed into powder, heated in reaction chamber in vac. at ca. 700 K for 2 h, temp. lowered to room temp., H2 put into reaction chamber in small portions in different alloy/H2 ratios; detd. by XRD, electron microscopy; content of hydrides depends on alloy/H2 ratio;
参考文献
Palewski; Tristan; Drulis; Cwik
Journal of Alloys and Compounds, 2005 , vol. 404-406, # SPEC. ISS. p. 584 - 587
in neat (no solvent)
compd. decompd. at 320-710°C with formation pyrolysis products - ZnCl2 and Ni; TGA, elem. anal.;
参考文献
Pirskii; Kublanovskii; Shevchenko; Kokozei
Russian Journal of Applied Chemistry, 2006 , vol. 79, # 12 p. 1964 - 1968
→
反应条件
in neat (no solvent)
byproducts: H2O, N2; mixt. of NiMoO4 and urea (molar raio 1:12) in an alumina boat placed in quartz tube and heated at 900°C for 3 h under N2; XRD;
参考文献
Gomathi