H2O; (C2H5)4NClO4 in further solvent(s) Electrolysis; electrolysis of CO2 in propylene carbonate contg. 0.1 M Et4NClO4 and 320 ppm of H2O /yield of CO depending on electrode material (95-100percent current efficiency on Sn at -2.4 V vs Ag/AgCl and In at -2.2--2.0 V, ca. 40percent on Zn electrode at -2.2 V); determined by gas chromy. and HPLC;
参考文献
Bulletin of the Chemical Society of Japan, , vol. 58, # 10 p. 3027 - 3028