反应条件
in neat (no solvent, solid phase) mixt. of NiO:V2O5:Cr2O3 in 65:15:20 molpercent ground, formed into pellets, heating in air in stages at 973-, 1073-, 1093 K for 24 h, after each heating stage samples homogenized, after fineal heating stage sloowly coolingdown to ambient temp., ground; Ni3V2O8 and NiCr2O4 can be produced by another initial mol ratios too;
参考文献
Rychlowska-Himmel; Bosacka
Journal of Physics and Chemistry of Solids, 2007 , vol. 68, # 5-6 p. 1193 - 1197