alumina catalyst (0.13 wtpercent Na2O, 0.35 wtpercent SiO2, specific surface area 391 m2/g, total pore volume 0.19 cc/g, pore volume of pores having a pore radius of at least 70 A is 74percent) in water T=360°C; P=2942.29 Torr; 5 - 800 h; Gas phase; Product distribution / selectivity;
ammonia; hydrogen; [RhCl(η2:η2-cycloocta-1,5-diene)]2; 2,2'-bis[[bis(3-sulfophenyl)phosphino]methyl]-4,4',7,7'-tetrasulfo-1,1'-binaphthyl octasodium salt in water T=100°C; P=47254.7 Torr; 7 h; Product distribution / selectivity;